Our Coatings



CoreHog's top-shelp coating options, including PCD, CVD, DLC, and others, are each specifically formulated to ensure your tool is fully equipped to manufacture composite materials more efficiently and accurately, providing you the best performance possible in your next CNC composite cutting application.



DLC

Image

 

Diamond-Like Coating
has extremely sharp
edges, improving
lubricity and wear
resistance in low
temperature threshold
applications of non-
ferrous materials.

 

Max. Working Temp
600° F

Microhardness (HV 0.05)
2,400 (24 GPa)

Coefficient of Friction
.05 - .1

Coating Thickness 
1 - 4 μm

Structure 
Mono-Layer

Color
Black

CVD

Image

 

True Crystalline
Diamond coating
is grown directly
onto a cutting tool,
dramatically improving
hardness, abrasion
resistance, and feed
rates in non-ferrous
machining applications.

 

Max. Working Temp
1,100° F

Microhardness (HV 0.05)
8,157-10,200 (80 - 100 GPa)

Coefficient of Friction
.05 - .30

Coating Thickness
4 μm Thinner CVD diamond layer provides a balance between wear resistance and edge sharpness.


12 μm Thicker diamond layer for increased wear resistance.

Structure
True Crystalline CVD Multi-Layer

Color
Gray

PCD

Image

 

Thick diamond layer
brazed onto solid
carbide body provides
outstanding micro
hardness and abrasion
resistance in low
temperature threshold
applications of non-
ferrous materials

 

Max. Working Temp
1,100° F

Microhardness (HV 0.05)
8,973 - 9,993
(88 - 98 GPa)

Coefficient of Friction
.05 - .20

Coating Thickness 
010” - .030” Solid PCD Layer

Structure 
Polycrystalline Diamond

Color
Gray / Black

ZrN

Image

 

Provides higher
hardness, lubricity,
and abrasion
resistance over
uncoated tooling
when machining a
variety of non-ferrous
materials.

 

Max. Working Temp
1,300° F

Microhardness (HV 0.05)
2,400 (24 GPa)

Coefficient of Friction
.30

Coating Thickness 
1 - 4 μm

Structure 
Mono-Layer

Color
Light Gold / Champagne

TiN

Image

 

High hardness general
purpose coating
improves overall tool
life and lubricity when
machining ferrous
materials and in
applications that do
not generate excessive
heat.

 

Max. Working Temp
1,100° F

Microhardness (HV 0.05)
2,400 (24 GPa)

Coefficient of Friction
.50

Coating Thickness 
1 - 7 μm

Structure 
Mono-Layer

Color
Gold

TiCN

Image

 

Maintains high
surface hardness and
increases abrasion
wear resistance to
improve overall tool life
in lower temperature
applications.

 

 

Max. Working Temp
750° F

Microhardness (HV 0.05)
3,500 (34 GPa)

Coefficient of Friction
.25

Coating Thickness 
1 - 4 μm

Structure 
Mono-Layer

Color
Gray / Silver